ABS resin injection molding processing points

2024-11-04 08:46:13 ABS
ABS resin injection molding requires attention to several key processing points:

1. Material Drying


  • Importance: ABS resin is hygroscopic. Moisture can cause bubbles in products during injection molding, reducing mechanical properties and causing surface defects like flow lines and silver streaks. It may also lead to material hydrolysis.

  • Conditions: The recommended drying temperature is 80 - 90 °C, which removes moisture without altering material properties. Drying time is usually 2 - 4 hours, but it should be adjusted based on initial moisture content, drying equipment efficiency, and environmental humidity, aiming for a moisture content below 0.1%.

2. Injection Temperature


  • Range Basis: The melting temperature of ABS is 220 - 260 °C, determined by its molecular structure and physical properties. In this range, the material can flow smoothly during injection.

  • Control Points

    • Barrel Temperature: It should increase from the rear to the front of the barrel. The rear end is 200 - 220 °C to prevent premature melting, and the front end near the nozzle is about 240 - 260 °C for complete melting. Stable temperature is crucial.

    • Nozzle Temperature: Usually 230 - 250 °C, matching the barrel front - end temperature. Too high a temperature may cause degradation, while too low may lead to nozzle clogging.


    injection mould


3. Injection Pressure


  • Selection Basis: ABS has higher melt viscosity than some other plastics due to its molecular structure. Higher injection pressure is usually needed, but for small, simple, and thick parts, lower pressure can be used.

  • Impact on Quality: Pressure at gate closure affects surface quality and silver - filament defects. Low pressure can cause atomization, while high pressure may lead to scratches, strains, and mold sticking.

4. Injection Speed


  • Selection Principle: Medium injection speed is generally best for ABS, ensuring smooth mold - cavity filling and reducing quality issues.

  • Impact on Quality

    • Too Fast: Can generate friction heat, causing plastic burning, decomposition, and defects like melting joints and poor luster. It may also suck air into the melt.

    • Too Slow: Unsuitable for thin - wall and complex parts, as it may result in short shots and insufficient filling due to rapid cooling of the melt.

5. Pressure and Time


  • Holding Pressure Setting: Increasing holding pressure can improve product shrinkage and internal quality, but too high pressure causes high internal stress. A lower holding pressure should be chosen, e.g., 50% - 70% of the initial injection pressure for high - requirement products.

  • Holding Time Setting: Based on the time when the gate cools and solidifies and the screw stops applying pressure. Too long time leads to excessive filling and high internal stress, while too short time causes shrinkage and size instability. The optimal time is when the product weight is unchanged.

6. Mold Temperature


  • Range and Function: The general mold temperature is 75 - 85 °C. For large - projection - area parts, the fixed mold temperature is 70 - 80 °C and the moving mold temperature is 50 - 60 °C. Higher mold temperature improves part flow, welding strength, and reduces internal stress but prolongs the cooling time.

  • Impact on Quality: Too low a mold temperature can cause high internal stress, reduced product performance, brittleness, and surface quality problems.

injection mould

7. Material Control


  • Influence of Quantity: When injecting ABS plastic, the injection volume is usually 75% of the standard volume to improve melt fluidity and distribution. To enhance part quality, a 50% calibration injection volume can be used, which also facilitates mold cleaning and maintenance.

  • Selection Basis: A smaller injection volume ensures smoother melt flow and filling, reducing quality issues.

8. Mold Design


  • Wall Thickness Uniformity: Product wall thickness should be uniform, with the wall - thickness difference of ABS products controlled within 25% to prevent stress concentration caused by uneven cooling and shrinkage.

  • Reinforcement Design: Add rounded corners or reinforcing bars to weak post roots to prevent breakage. Fastener roots should also be rounded, with the r - angle to wall - thickness ratio above 0.3, considering surface shrinkage.

  • Cooling Water Design: The mold cooling waterway should ensure uniform cooling to avoid internal stress and uneven shrinkage, especially for complex - shaped products.

injection mould


Home
Product
News
Contact
主站蜘蛛池模板: 精品精品国产高清a级毛片| 出租屋勾搭老熟妇啪啪| 无码丰满少妇2在线观看| 国产欧美一区二区三区在线看| 最好免费观看高清视频大全| 久久香蕉国产线看观看精品yw| 成全电影大全免费观看完整视频| 午夜人妻久久久久久久久| 无码精品a∨在线观看中文 | 五月综合激情婷婷六月色窝| 99久久精品费精品国产| 日本丰满岳乱妇在线观看| 亚洲av成人一区二区三区在线播放| 天天色影网| 男人的天堂av社区在线| 少妇特殊按摩高潮惨叫无码| 日韩精品无码熟人妻视频| 艳妇臀荡乳欲伦交换在线播放| 男人扒开女人双腿猛进视频 | 国产精品日本一区二区在线播放| 亚洲欧美日韩国产精品专区| 精品成在人线av无码免费看| 999在线视频精品免费播放观看| 国产精品久久久久av| 亚洲a无码综合a国产av中文| 亚洲欧洲自拍拍偷午夜色无码| 柠檬福利第一导航在线| 久久66热人妻偷产精品| 欧美变态口味重另类在线视频| 成人片在线观看地址kk4444| 欧美日韩精品乱国产| 国产偷窥熟女精品视频| 欧美黑人又粗又大久久久| 天天狠天天透天干天天怕∴| 欧美巨大巨粗黑人性aaaaaa| 嫖妓丰满肥熟妇在线精品| 国产精品毛片在线完整版| 成人免费一区二区三区| 免费不卡在线观看av| 欧美日韩国产精品| 国产成人亚洲综合无码精品|